Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Index of Compound 4.0 - 6.0 g/10 min
4.0 - 6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 101
101
ASTM D785
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Flexural Yield Strength 98.1 MPa
14200 psi
ASTM D790
Izod Impact, Notched 3.92 J/cm
7.35 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648