Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic A702G15 ABS 15% Glass Fiber Reinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic A702G15 ABS 15% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102
102
ASTM D785
Tensile Strength, Yield 66.9 MPa
9700 psi
ASTM D638
Flexural Yield Strength 118 MPa
17100 psi
ASTM D790
Izod Impact, Notched 1.35 J/cm
2.53 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648
Flammability, UL94 HB
HB