Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 104-13 G Nylon 66, 13% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 104-13 G Nylon 66, 13% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A toughened, 13% glass fiber reinforced nylon 66 exhibiting improved toughness and ductility, especially dry as molded.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ASTM D638
Elongation at Break 4.6 %
4.6 %
ASTM D638
Flexural Yield Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 3.80 GPa
551 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 279 °C
534 °F