CTC X-PRO CF 40 6002XT Polypropylene Copolymer, 40% Calcium Carbonate Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer CTC (Composite Technologies)
Trade Name X-PRO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CTC X-PRO CF 40 6002XT Polypropylene Copolymer, 40% Calcium Carbonate Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
X-PRO CF 40 6002 XT is a heat stabilized, 40% calcium carbonate filled polypropylene copolymer. It has an application in extrusion.Data provided by Composite Technologies (CTC).
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM-D792
Filler Content 40 %
40 %
Calcium Carbonate; ASTM-D5630
Melt Flow 1.0 - 5.0 g/10 min
1.0 - 5.0 g/10 min
ISO 1133/ASTM-D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM-D638
Flexural Modulus 1.72 GPa
250 ksi
Secant; ASTM-D790
2.41 GPa
350 ksi
Tangent; ASTM-D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM-D256
Descriptive Properties Value Comments
Color General Purpose Black