Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carpenter Glass Sealing "42-6" Alloy

Category Metal , Electronic/Magnetic Alloy , Ferrous Metal , Superalloy
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter Glass Sealing "42-6" Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A nickel-chromium-iron which has been developed to match the thermal expansion characteristics of 0120 glass. An additional advantage of this alloy for glass-to-metals seals is the tight dark green oxide coating formed by wet hydrogen annealing at 1900/2200°F (1038/1204°C) for one hour. The oxide tends to flux with the glass and make it a vacuum tight seal if the surfaces are clean. To obtain the necessary surface cleanliness, pickle in muriatic acid.This alloy has been supplied in strip form for glass windows and television/CRT anode buttons. It is supplied in wire form for compression seals.Data provided by Carpenter Technology Corporation.
Physical Properties Metric English Comments
Density 8.11 g/cc
0.293 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 159 GPa
23000 ksi
Thermal Properties Metric English Comments
CTE, linear 2.02 µm/m-°C

@Temperature 25.0 - 100 °C
1.12 µin/in-°F

@Temperature 77.0 - 212 °F
2.19 µm/m-°C

@Temperature 25.0 - 200 °C
1.22 µin/in-°F

@Temperature 77.0 - 392 °F
Specific Heat Capacity 0.502 J/g-°C
0.120 BTU/lb-°F
Thermal Conductivity 12.5 W/m-K
86.8 BTU-in/hr-ft²-°F
Melting Point 1427 °C
2601 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.070 %
<= 0.070 %
Chromium, Cr 5.75 %
5.75 %
Iron, Fe 51 %
51 %
as remainder
Manganese, Mn 0.50 %
0.50 %
Nickel, Ni 42.5 %
42.5 %
Silicon, Si 0.25 %
0.25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000948 ohm-cm
0.0000948 ohm-cm
Curie Temperature 293 °C
559 °F
Copyright © lookpolymers.com All Rights Reserved