Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scratch resistance. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Melt Flow 15 - 20 g/10 min

@Temperature 230 °C
15 - 20 g/10 min

@Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 86
86
ASTM D785
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
ASTM D648