Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 2.02 µm/m-°C @Temperature 25.0 - 100 °C |
1.12 µin/in-°F @Temperature 77.0 - 212 °F |
|
Carpenter Glass Sealing "42-6" Alloy A nickel-chromium-iron which has been developed to match the thermal expansion characteristics of 0120 glass. An additional advantage of this alloy for glass-to-metals seals is the tight dark green.. |