Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.11 g/cc | 0.293 lb/in³ | |
Lucas-Milhaupt SIL-FOS 18 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 18 is a moderate cost brazing filler metal suitable for joining copper, brass and bronze alloys where low brazing temperature and free flowing characteristics are required. I.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals INCONEL® 601GC® Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals INCONEL® Alloy 601 A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals NILO® 365 Controlled-Expansion Alloy For the manufacture of tooling for composites, the NILO® nickel-iron alloys offer a unique combination of matched thermal expansion to avoid warping during the curing cycle, along with strength, .. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals NILO® Alloy 36 Low-Expansion Alloy Inflection point 220°C. A nickel-iron low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coeffic.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Crucible Steel CPM® REX® M35HCHS High Speed Steel, AISI M35 CPM REX M35HCHS is a 5% cobalt modification of M2 high speed steel used almost exclusively for hobs and other gear cutting tools where higher red hardness is required. Made by the Crucible Particle .. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
California Fine Wire Stablohm 800 Nickel, Chromium, Aluminum, and Copper Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Carlson C 601 Nickel-Chromium-Iron Alloy General DescriptionCarlson Alloy C 6021 is a nickel-chromium alloy, developed specifically for high –temperature service. This alloy exhibits outstanding resistance to both cyclic and static oxida.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
ATI Allvac® Nickelvac® N-90 Nickel Superalloy, Heat Treatment: 1066°C (1950°F) + Age Data provided by Allvac.Applications: Turbine blades and other jet engine components. Valves for internal combustion engines. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Carpenter Glass Sealing "42-6" Alloy A nickel-chromium-iron which has been developed to match the thermal expansion characteristics of 0120 glass. An additional advantage of this alloy for glass-to-metals seals is the tight dark green.. |