Pau Tai UNISTAB BTM-17 Organo Tin Stabilizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name UNISTAB
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai UNISTAB BTM-17 Organo Tin Stabilizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent clarity,heat stability and color retention.Very effective of copolymer or for formulation involving PVC with ABS and NBR.For flexible and rigid PVC articles processed by calendering,extrusion,and molding.Information provided by Pau Tai Industrial Corp.