Carmel Olefins IPETHENE® 810 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Carmel Olefins
Trade Name IPETHENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins IPETHENE® 810 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IPETHENE® 810 is a low density polyethylene injection molding grade. It exhibits high melt flow rate, high gloss, and high stiffness. APPLICATIONS IPETHENE® 810 is used to produce lids, containers, toys, and domestic hollowware.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ISO 1183-A
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.5 MPa
1520 psi
ISO 527-2
Tensile Strength, Yield 10.5 MPa
1520 psi
ISO 527-2
Elongation at Break 130 %
130 %
ISO 527-2
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C

@Load 1.02 kg
187 °F

@Load 2.25 lb
ISO 306