Polymer Property : Tensile Strength, Ultimate = 53.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.8 - 103 MPa
7800 - 15000 psi
Average value: 83.6 MPa Grade Count:25
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Tensile Strength, Ultimate 53.8 MPa
7800 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® NJ-000/000 Nylon 12  (discontinued **)
Description/Features:General Purpose GradeHeat StabilizedHigh FlowUL 94 HBProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 53.8 MPa
7800 psi
ASTM D638
Styron Pulse® 2100LG ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 53.8 MPa
7800 psi
Williams Advanced Alloys WS186 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Tensile Strength, Ultimate 53.8 MPa
7800 psi
ASTM D638
CPC - Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
Flametec™ Halar® ECTFE (Ethylene Chlorotrifluoroethylene) is an ultra-pure fluoropolymer that is a tough engineering thermoplastic with a balance of physical and chemical properties that qualify i..
Tensile Strength, Ultimate 53.8 MPa
7800 psi
Very Dry (Desiccated)
AdvanSource Biomaterials HYDROTHANE™ Hydrophilic Thermoplastic Polyurethane
AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether aliphatic polyurethanes designed for use as coatings of catheters, sutures, intr..
Tensile Strength, Ultimate 53.8 MPa
7800 psi
BCC Products BC 5200 Kwik-Set Adhesive
BC5200 is a medium viscosity fast gelling two part Epoxy Adhesive System. With an easy to use 1 to 1 mix ratio, BC5200 is considered an excellent general purpose adhesive for in-shop use. BC5200 wil..
Tensile Strength, Ultimate 53.8 MPa
7800 psi
Abatron AboCast 7703-21/AboCure 7703-23 (C) Epoxy Adhesive and Casting Compound
AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane..
Tensile Strength, Ultimate 53.8 MPa
7800 psi
BCC Products BC 7136 Epoxy Casting
BC7136 is a gray, low toxicity, aluminum filled, epoxy casting resin. This heat resistant system may be used at room temperature without post-curing. May be cast to a thickness of ¾ inch in non-con..
Tensile Strength, Ultimate 53.8 MPa
7800 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PE-25CF/000 High Density Polyethylene (HDPE), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.