Material Notes:
Description: Formulated with PVC, it is used in in the production of stretch film for food contact.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Viscosity 2500 - 3000 cP

@Temperature 35.0 °C
2500 - 3000 cP

@Temperature 95.0 °F
Dynamic viscosity
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
Tensile Strength, Yield 26.06 MPa
3780 psi
Elongation at Break 275 %
275 %
100% Modulus 0.00909 GPa
1.32 ksi
Optical Properties Metric English Comments
Gardner Color Number 2.0
2.0
Chemical Properties Metric English Comments
Acid Value 2.0
2.0
mgKOH/g
Descriptive Properties Value Comments
Efficiency concentration PHR 33.5
N OH value (max) 75
mg KOH/g
N OH value (min) 70
mg KOH/g