Wanshijie PC Film

Category Polymer , Film , Thermoplastic , Polycarbonate (PC)
Manufacturer Wanshijie Plastic Sheet Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanshijie PC Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC is a kind of shapeless, odorless, non-toxic, high transparency, colorless or light yellow thermoplastic engineering plastic with excellent physical and mechanical properties, especially excellent impact resistance, high tension strength, high bending strength, high compression strength, high creep resistance and stable clemencies It also has good heat resistance and low temperature resistance, Within a wide temperature range it has stable mechanical properties, dimensional stabilities, electrical properties and flame redundancy. It can be used at -60~120°C for a long time without an obvious melting paint and it becomes to be the melting state at 220-230°C, the rightist of molecular chain is high, so the viscosity of resin melt is high It has low water absorption and shrinkage, and high precision dimensions and low permeability. It is stable when subject to light but can not withstand UV. It is resistant to oil and acid, but not resistant to strong alkali, oxidizing acid, ketene and amine. It can be dissolved in chlorinated hydrocarbon and aromatic solvent. It can be hydrolyzed and cracked when put in the water for a long time. The disadvantages of it are poor fatigue stress, poor solvent resistance and poor wearing resistance.MAIN APPLICATIONS: automobile industry, electronic and electrical appliances industries, LCD and mechanical parts, plating lens, various labels, prints, film switches, chrome plates, arc-protection helmets/glass assembly industries, industrial machine accessory, discs, packing, computer and simliar office equipments, medical treatment and health care, film, leaisure and protection equipments.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption <= 0.40 %
<= 0.40 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 55.0 MPa
>= 7980 psi
ASTM D882
Elongation at Break >= 90 %
>= 90 %
ASTM D882
Tensile Modulus 2.00 GPa
290 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
ASTM D117
Vicat Softening Point 135 °C
275 °F
ASTM D1525
Brittleness Temperature -130 °C
-202 °F
ASTM D746
Flammability, UL94 V-2

@Thickness 0.250 mm
V-2

@Thickness 0.00984 in
Shrinkage <= 0.30 %

@Temperature 135 °C
<= 0.30 %

@Temperature 275 °F
ASTM D1204
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D495
Surface Resistivity per Square >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Dielectric Constant 2.95

@Frequency 1e+6 Hz
2.95

@Frequency 1e+6 Hz
ASTM D150
2.98

@Frequency 60 Hz
2.98

@Frequency 60 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm
762 kV/in
Short Time; ASTM D149
Arc Resistance >= 100 sec
>= 100 sec
ASTM D495