Material Notes:
High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 0.25 %
0.25 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength at Break 97.9 MPa
14200 psi
ASTM D882
Elongation at Break 52 %
52 %
ASTM D882
Tensile Modulus 3.28 GPa
475 ksi
ASTM D882
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Tear Strength 147 kN/m
840 pli
ASTM D1004
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 170 °C
338 °F
Continuous Use
Deflection Temperature at 1.8 MPa (264 psi) 201 °C
394 °F
ASTM D648
Glass Transition Temp, Tg 215.5 °C
419.9 °F
ASTM D3418
Flammability, UL94 V-0
V-0
VTM-0
NBS Smoke Density <= 6.0
<= 6.0
ASTM E662
Oxygen Index 47 %
47 %
ASTM D2863
Optical Properties Metric English Comments
Refractive Index 1.658
1.658
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+16 ohm
>= 1.00e+16 ohm
ASTM D257
Dielectric Constant 3.15

@Frequency 1000 Hz
3.15

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 120 kV/mm

@Thickness 0.0762 mm
3050 kV/in

@Thickness 0.00300 in
ASTM D149
Dissipation Factor 0.0013

@Frequency 1000 Hz
0.0013

@Frequency 1000 Hz
ASTM D150