Material Notes:
Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life. The sulfur-phosphorus extreme pressure additives used in Havoline Gear Oils provide superior thermal and oxidation stability.Recommended for use in all spiral bevel and hypoid differentials, power dividers, and oil lubricated steering axle wheel bearings. The multiviscosity characteristics allow use in equipment operating over a broad ambient temperature range. Havoline Gear Oils meet the performance requirements of API Service Categories MT-1 and GL-5, MIL-PRF-2105E, Mack GO-J, USDA H2.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 222272; MSDS Number: 8600
Physical Properties Metric English Comments
API Gravity 25.9 °
25.9 °
Brookfield Viscosity 102000 cP

@Temperature -12.0 °C
102000 cP

@Temperature 10.4 °F
Viscosity Measurement 95
95
Viscosity Index
Saybolt Viscosity at 100°F 1819 SUS
1819 SUS
Saybolt Viscosity at 210°F 124 SUS
124 SUS
Kinematic Viscosity at 40°C (104°F) 341 cSt
341 cSt
Kinematic Viscosity at 100°C (212°F) 25 cSt
25 cSt
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
ASTM D 2783
Timken Test 29500 g
65.0 lb
OK Load
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flash Point 229 °C
444 °F
Descriptive Properties Value Comments
Load Weld Index, kg 50
ASTM D 2783