Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.12 - 1.19 g/cc | 0.0405 - 0.0428 lb/in³ | |
CMT Materials HYTAC® B Solid Polymer Tooling Material Sometimes, finer plug assist details are required which are not obtainable or maintainable with syntactic foam plugs. For these high detail applications, where high toughness and easy machinability .. |