Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Buckeye Polymers BP PPC 0212 BLK Polypropylene Copolymer

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP PPC 0212 BLK Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resistanceHigher melt flow available for improved processibilityAppearance: BlackForms: PelletsRecycled Content: NoProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.880 - 0.910 g/cc
0.880 - 0.910 g/cc
ASTM D792
Linear Mold Shrinkage 0.017 - 0.018 cm/cm
0.017 - 0.018 in/in
ASTM D955
Melt Flow 8.0 - 14 g/10 min
8.0 - 14 g/10 min
ASTM D1238
Ash <= 5.0 %
<= 5.0 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 18.6 MPa
>= 2700 psi
ASTM D638
Flexural Modulus >= 1.07 GPa
>= 155 ksi
ASTM D790
Izod Impact, Notched >= 0.934 J/cm
>= 1.75 ft-lb/in
ASTM D256