Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.880 g/cc | 0.880 g/cc | |
Radici Heraflex® A 55 I RKT TPS-SEBS Thermoplastic Elastomer Shore hardness: 55A (3s)Transparent, scratch resistant and high heat resistanceApplication examples: soft touch, housewares, tool handles, toys, PP overmoldingInformation provided by Radici group. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | 20/20°C |
LyondellBasell PNB Propylene glycol normal butyl ether Information provided by Lyondell. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 2111 Thermoplastic Elastomer Uses: Grips Features: Excellent Resistance to Skin OilsInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1564L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1580L1-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1775 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1775A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1775B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2111S-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2238-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1580L1 Thermoplastic Elastomer Notes: USP Class VI; Translucent Features: High Throughput Uses: Medical TubingInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1644 Thermoplastic Elastomer Notes: Clear Features: High Flow; High Coefficient of FrictionInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1437A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2830C CLR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Telcar® OBC 2318D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Telcar® OBC 4565A Thermoplastic Elastomer Uses: Flexible Grips; Overmolding Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion; Extrusion; Injection Molding Injection .. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ISO 1183/1 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ISO 1183/1 |
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ISO 1183/1 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | 15°C; ASTM D4052 |
ExxonMobil 446 Mobilmet 440 Series Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ISO 1183/1 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ISO 1183/1 |
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D1298 |
ExxonMobil Mobilarma 778 The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte.. |
|||
Specific Gravity | 0.880 g/cc @Temperature 25.0 °C |
0.880 g/cc @Temperature 77.0 °F |
|
Dow Corning Z-6224 SILANE Dow Corning® Z-6224 Silane contains vinylbenzyl and amine organic groups and methoxysilyl inorganic reactivity. The product is supplied in methanol. It is the neutralized (low chloride) version of .. |
|||
Specific Gravity | 0.880 - 0.910 g/cc | 0.880 - 0.910 g/cc | ASTM D792 |
Buckeye Polymers BP PPC 0212 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2854T Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ISO 2782 |
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
G-2712 Styrene-based Biomedical Elastomer |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2830M UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |