Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1843L1 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1869 Thermoplastic Elastomer Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1564L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1580L1-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1736R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1797 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1870-CR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2111S-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2287 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2315C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1304 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1595 Thermoplastic Elastomer Features: Nice Silken Feel Uses: Leisure ProductsInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP 1736R Thermoplastic Elastomer Notes: Soft Material; Overmold onto PP handlesInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2840M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Telcar® OBC 4955A Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Telcar® OBC 4965A Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | 15°C; ASTM D4052 |
ExxonMobil 446 Mobilmet 440 Series Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | 15°C; ASTM D1298 |
ExxonMobil 766 Mobilmet 760 Series Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ISO 1183/1 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D1298 |
ExxonMobil Mobilarma 778 The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte.. |
|||
Specific Gravity | 0.880 g/cc @Temperature 25.0 °C |
0.880 g/cc @Temperature 77.0 °F |
|
Dow Corning Z-6224 SILANE Dow Corning® Z-6224 Silane contains vinylbenzyl and amine organic groups and methoxysilyl inorganic reactivity. The product is supplied in methanol. It is the neutralized (low chloride) version of .. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | Part B |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Specific Gravity | 0.880 - 0.910 g/cc | 0.880 - 0.910 g/cc | ASTM D792 |
Buckeye Polymers BP PPC 0212 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2854T Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
E-Polymers EFLEX® S2040 Transparent S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplas.. |
|||
Specific Gravity | 0.880 g/cc | 0.880 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2830M UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |