Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.4699 - 0.94975 GPa | 68.15 - 137.75 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D5512 RU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Flexural Modulus | 0.4699 - 0.94975 GPa | 68.15 - 137.75 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D5518 R 848 Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |