Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.1 MPa | 1470 psi | ASTM D412 |
Polymax® Maxelast® A9750 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 10.1 MPa | 1460 psi | ASTM D412 |
Polymax® Maxelast® A9860M TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 10.1 MPa | 1460 psi | At 100% elongation, across flow; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength, Yield | 10.1 MPa | 1460 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7727 HM Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 10.1 MPa | 1470 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3310-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | >= 10.1 MPa | >= 1470 psi | ASTM D638 |
Buckeye Polymers BP FLEX D5512 RU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | 10.1 MPa | 1470 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3880E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |