Material Notes:
Description: High Melt Flow, Nucleated, Excellent Mold Release, AntistaticApplications: Suggested Uses Include Housewares, Large Part Injection Molding, Thin-Walled Injection MoldingThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 20.7 MPa
3000 psi
2 in/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256A