AdvanSource Biomaterials HYDROTHANE™ Hydrophilic Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer AdvanSource Biomaterials (formerly CardioTech International)
Trade Name HYDROTHANE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AdvanSource Biomaterials HYDROTHANE™ Hydrophilic Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether aliphatic polyurethanes designed for use as coatings of catheters, sutures, introducers, rods, valves and rubber products. Hydroslip C polymers can also be coated onto silicon microdevices to reduce absorption of white cells and proteins on the devices, thereby aiding in the analysis of blood and DNA.Information provided by AdvanSource Biomaterials Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A <= 85
<= 85
Wet (24 Immersion)
<= 93
<= 93
Very Dry (Desiccated)
<= 95
<= 95
In Normal Atmosphere
Tensile Strength, Ultimate 38.6 MPa
5600 psi
Wet (24 Immersion)
40.0 MPa
5800 psi
In Normal Atmosphere
53.8 MPa
7800 psi
Very Dry (Desiccated)
Elongation at Break 475 %
475 %
In Normal Atmosphere
500 %
500 %
Wet (24 Immersion)
580 %
580 %
Very Dry (Desiccated)
Processing Properties Metric English Comments
Zone 1 170 °C
338 °F
Zone 2 185 °C
365 °F
Zone 3 190 °C
374 °F
Melt Temperature 175 °C
347 °F
Drying Temperature 85.0 °C
185 °F
Dry Time >= 3 hour
>= 3 hour
Moisture Content <= 0.10 %
<= 0.10 %
Dew Point -5.00 °C
23.0 °F