Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Pro® 1010 C Natural 10% Filler Content Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 1010 C Natural 10% Filler Content Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955-89
Melt Flow 10 g/10 min
10 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 29.4 MPa
4260 psi
ASTM D638-95
Elongation at Break 686 %
686 %
ASTM D638-95
Flexural Strength 38.1 MPa
5530 psi
ASTM D790-95
Flexural Modulus 1.441 GPa
209.0 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256-93a
Gardner Impact 5.10 J
3.76 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648-95