Material Notes:
Description: H 605 is a low melt flow rate homopolymer with high transparency. This resin is designed for extrusion and thermoforming. H 605 exhibits excellent processability, high output, excellent stiffness/impact strength balance, high melt strength, outstanding optical properties and low odor/taste transfer. Applications: Highly transparent thermoformed packages for food, cosmetic, health care and cleaning products; Flat and corrugated sheets for school and office folders Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
10 N; ASTM D1525
Optical Properties Metric English Comments
Haze 30 %
30 %
ASTM D1003
Users viewing this material also viewed the following: