Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 37.0 - 126 MPa | 5370 - 18300 psi | Average value: 59.7 MPa Grade Count:49 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Ineos ABS Lustran® 1148 General Purpose, High-Impact
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50 mm/min |
Polimeri Europa SINKRAL PD G523 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-25-20 High impact injection moulding grade. Other characteristics: good flow, excellent thermal stabilit.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50 mm/min |
Eastman Tenite 383A-08 Cellulose Acetate Propionate
(discontinued **) 8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills P4G4A-053 Polypropylene Homopolymer Features: Good stiffness, long term heat aging (LTHA). Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: High heat resistanceInformation Provided .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638-02 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
IRPC Polimaxx Polene 1102H Polypropylene Homopolymer CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS: MONOFILAMENT/YARN/SHEET EXTRUSION FOR THERMOFORMINGBLOW MOLDING AND INJECTION MOLDING FOR ROPESCOARSE TEXTILE FOR JUMBO .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50mm/min; ISO 527-1/-2 |
Styrolution Terluran® SP-6 ABS Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP Stat-loy W3000 PBT LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | SABIC - Japan Method |
SABIC Innovative Plastics Noryl EUN0240 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Teknor Apex Sinpolene TPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 40% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Denka MALECCA K-600 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437G20M10CL Glass/Mineral Reinforced Coupled |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50 mm/min |
Arkema Group Rilsan® BESVO A FDA Nylon 11 (Conditioned) Designation ISO 1874-PA11,E,22-010Rigid grade for tubes and films extrusion in food applications. Available color: natural. Additive free.Good thermal and chemical resistance. Transparency. Barrier .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336M30CL Mica Reinforced Coupled |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific) LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
Unipetrol PP MONSTEN® FK 005 Polypropylene Homopolymer Applications include injection molding and thermoforming. Antistatic stabilized. Homopolymer.Information provided by Unipetrol RPA |