Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills H0500HN Polypropylene Homopolymer Features: Nucleated and long term heat aging (LTHA). Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: medical partsInformation Provided by Flint .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills P4C5B-076 Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: cutlery and closuresFormer Huntsman polypropylene products are now produced by .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Flint Hills P4G2Z-159 Polypropylene Homopolymer Features: High xylene soluble. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: BOPP FilmInformation Provided by Flint Hills Resources |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM-D638 |
Ineos ABS Lustran® 266 ABS, Transparent Grade Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing... |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Ineos H13M-00 Polypropylene Homopolymer Grade H13M-00 is a general purpose polypropylene homopolymer for injection molding applications. It provides good long-term heat stability.Suggested fabrication methods: Injection moldingFeatures: .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
IRPC Polimaxx Polene 1102H Polypropylene Homopolymer CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS: MONOFILAMENT/YARN/SHEET EXTRUSION FOR THERMOFORMINGBLOW MOLDING AND INJECTION MOLDING FOR ROPESCOARSE TEXTILE FOR JUMBO .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp ZI001 PPO LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
SABIC Innovative Plastics LNP Stat-loy W3000 PBT LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Total PPH 12020 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 12020 is a clarified high fluidity homopolymer with a melt flow index of 60 g/10 min.Polypropylene PPH 12020 has been designed with a very high stiffness and an outstanding transpa.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Total PPH 3740WR Polypropylene, High Flow Nucleated Homopolymer Injection Molding Easy Flow TOTAL Polypropylene 3740WR exhibits exceptionally easy flow characteristics.FDA. 3740WR complies with all applicable FDA and USDA regulations and may be used under these provisions for .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527-2 |
Denka MALECCA K-700 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO R 527 |
Addiplast Addilene H 560 Polypropylene Homopolymer High heat resistance, detergent stabilized, anti-yellowingInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | 50 mm/min |
Arkema Group Orgalloy® LE 60ES Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in viscosity than LE 6000, suited to the blow molding of tec.. |
|||
Tensile Strength, Yield | 37.0 - 154 MPa | 5370 - 22300 psi | Average value: 63.3 MPa Grade Count:371 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Eastman Tenite Acetate 109E3V36324 Clear, Trsp Cellulose Acetate
(discontinued **) Plasticizer 24%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
Braskem H 501HC Thermoforming Polypropylene Homopolymer High-stiffness thermoformed parts.Information provided by Braskem. |
|||
Tensile Strength, Yield | 37.0 MPa | 5370 psi | ISO 527 |
Unipetrol PP MONSTEN® FK 005 Polypropylene Homopolymer Applications include injection molding and thermoforming. Antistatic stabilized. Homopolymer.Information provided by Unipetrol RPA |