Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.1 MPa | 1610 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2165 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 11.1 MPa | 1610 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Tensile Strength at Break | >= 11.1 MPa | >= 1610 psi | after aging (168h, 150°C); ASTM D412 |
Borealis PC0798 Polyethylene Insulation Compound, Crosslinkable PC0798 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0798 is a halogenated, colorable, chemically crosslinkable copolymer compound which contains flame retar.. |
|||
Tensile Strength at Break | 11.1 MPa | 1610 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 11.1 MPa | 1610 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Strength at Break | 11.1 MPa | 1610 psi | ISO 37 |
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 11.1 MPa | 1610 psi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2160 BK Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
Tensile Strength at Break | 11.1 MPa | 1610 psi | ISO 37 |
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 11.1 MPa | 1610 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |