Electrical Properties Metric English Comments
Dielectric Strength >= 550 kV/mm
>= 14000 kV/in
ASTM D149
Borealis PC0787 Polyethylene Insulation Compound, Crosslinkable
PC0787 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0787 contains flame retardant additives to reduce normal flame spread characteristics so as to achieve a..
Dielectric Strength >= 550 kV/mm
>= 14000 kV/in
ASTM D149
Borealis PC0798 Polyethylene Insulation Compound, Crosslinkable
PC0798 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0798 is a halogenated, colorable, chemically crosslinkable copolymer compound which contains flame retar..