Material Notes:
LE1169 is a low loss LDPE compound for coaxial cables. LE1169 contains a special type of antioxidant, which does not adversely affect the electrical properties. Applications: coaxial cables Specifications: LE1169 meets the applicable requirements as below when processed using sound extrusion practice and testing procedure: ASTM D1248 Type I, Class A, Category 3, Grade E1, E2, E3; BS 6234: Type 2; and ISO 1872-PE, KHN, 23-D022.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
1s; ISO 868
Tensile Strength at Break 13.0 MPa
1890 psi
50mm/min; ISO 527
Elongation at Break 600 %
600 %
50mm/min; ISO 527
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+6 ohm-cm
<= 1.00e+6 ohm-cm
IEC 60093
Dielectric Constant 2.28

@Frequency 1.00e+6 Hz
2.28

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
559 kV/in
IEC 60243
Dissipation Factor 0.000090

@Frequency 1.00e+6 Hz
0.000090

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 160 - 190 °C
320 - 374 °F