Material Notes:
Casico™ FR6083 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, UV stabilized, natural jacketing compound combining with excellent extrusion properties. The composition is based on the elements Carbon, Hydrogen, Oxygen, Silicon and Calcium. Compounds based on these elements will therefore be the only significant constituents of the combustion fumes. Other elements may be present in concentrations less than 0.1%. Applications: jacket for energy cables. The principal feature of this compound is the high physical strength and toughness. It can be used in areas sensitive to smoke or corrosive and toxic combustion products. For most cable constructions, Casico™ FR6083 has sufficient flame retardancy to satisfy single wire vertical burning tests. Specifications: HD 603 S1; EN 50363-8; IEC 60840, Type ST7; IEC 60502, Type ST7; and IEC 60502, Type ST8Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1872-2/ISO 1183
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
15s; ISO 868
Tensile Strength at Break 2.25 MPa
326 psi
after aging, 240h, 100°C; or UV aging; IEC 60811-1-2
15.0 MPa
2180 psi
50mm/min; IEC 60811-1-1
Elongation at Break 75 %
75 %
after aging, 7h, 110°C; IEC 60811-1-2
500 %
500 %
IEC 60811-1-1
Thermal Properties Metric English Comments
Oxygen Index 28 %
28 %
ISO 4589A
Electrical Properties Metric English Comments
Volume Resistivity 1.80e+6 ohm-cm
1.80e+6 ohm-cm
IEC 60093
Processing Properties Metric English Comments
Zone 1 160 °C
320 °F
Zone 2 170 °C
338 °F
Zone 3 180 °C
356 °F
Zone 4 190 °C
374 °F
Die Temperature 190 °C
374 °F
Descriptive Properties Value Comments
High Temperature Pressure Test, % 15
110°C, 6h; IEC 60811-3-1
5
105°C, 6h; IEC 60811-3-1
Single Vertical Flame Test Pass
IEC 602431