Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.80e+6 ohm-cm | 1.80e+6 ohm-cm | IEC 60093 |
Borealis Casico™ FR6083 Reduced Fire Hazard Jacketing Compound Casico™ FR6083 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, UV stabilized, natural jacketing compound combining with excellent extrusion properties. The composition is based o.. |