Borealis Borpact™ BC918CF Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Borpact™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borpact™ BC918CF Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borpact™ BC918CF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. Optical properties will not be deteriorated as with conventional homo or copolymers at these temperatures. This grade is especially developed for the manufacturing of unoriented film for various film processing technologies like cast film process, conventional blown film process with air cooling and roll stack process for thermoformable films/sheets. Applications: Borpact™ BC918CF is designed for label film, lamination films, food packaging, stand up pouch film, inner layer in coextrusion, map trays, and vegetable trays.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Flexural Modulus 1.40 GPa
203 ksi
50% humidity; ISO 178
Charpy Impact, Notched 0.230 J/cm²

@Temperature -20.0 °C
1.09 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
DSC; ISO 3146
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb
A50; ISO 306