Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.230 J/cm² @Temperature 23.0 °C |
1.09 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PH 52 T 20 003/1M Polypropylene reinforced with 20% mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature 23.0 °C |
1.09 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PH 91 SDU Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature 23.0 °C |
1.09 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature 23.0 °C |
1.09 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B1 GF 10 FRX 5 PBT reinforced with 10% glass fibre, with flame retardant Features: PBT with the content of 10 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho.. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature -30.0 °C |
1.09 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A CV300LK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature 23.0 °C |
1.09 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature -20.0 °C |
1.09 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-3810 10% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-3810 is a 10% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-3810 is recommended for producing in.. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature -20.0 °C |
1.09 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle.. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature 23.0 °C |
1.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-1120 AN 20% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-1120 AN is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-1120 AN is develo.. |
|||
Charpy Impact, Notched | 0.230 J/cm² @Temperature -20.0 °C |
1.09 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Borpact™ BC918CF Polypropylene Copolymer Borpact™ BC918CF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. Optical properties will not be deteriorated as with conventional homo or .. |