Borealis Bormed™ RD808CF Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Bormed™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ RD808CF Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed™ RD808CF is a random copolymer. Applications: Bormed™ RD808CF is intended for packaging for medical devices, thin pouches, and packaging for pharmaceutical products. Additives: Bormed™ RD808CF contains no slip, antiblock, antistatic additives or nucleating additivesInformation provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 0.400 GPa
58.0 ksi
MD/TD; ISO 527-3
Flexural Modulus 0.700 GPa
102 ksi
50% humidity; ISO 178
Dart Drop, Total Energy 30.0 J

@Thickness 0.0500 mm
22.1 ft-lb

@Thickness 0.00197 in
1100N; ISO 7765-2
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ISO 527-3
Film Tensile Strength at Break, TD 30.0 MPa
4350 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 140 °C
284 °F
DSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ISO 75-2
Vicat Softening Point 125 °C

@Load 1.02 kg
257 °F

@Load 2.25 lb
ISO 306
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Gloss >= 150 %
>= 150 %
20° of arc; ASTM D2457