Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG47 ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG47F ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific) CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla.. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® DMX3415M PC Copolymer (Europe-Africa-Middle East) Lexan* DMX3415M is a co-polycarbonate resin with improved scratch and abrasion resistance compared to standard polycarbonate. Lexan* DMX3415M is available in transparent colors. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Dart Drop, Total Energy | 30.0 J | 22.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 30.0 J | 22.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific) LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HFD4472 PC (Asia Pacific) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Dart Drop, Total Energy | 30.0 J | 22.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |
|||
Dart Drop, Total Energy | 30.0 J | 22.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC (Asia Pacific) LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
Dart Drop, Total Energy | 30.0 J | 22.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC (Asia Pacific) LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM UF5011S PEI Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dart Drop, Total Energy | 30.0 J | 22.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEF42 PC (Asia Pacific) LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Europe-Africa-Middle East) high gloss Noryl |
|||
Dart Drop, Total Energy | 30.0 J | 22.1 ft-lb | 900N; ISO 7765-2 |
Borealis Borseal™ RE939CF Polypropylene Copolymer Borseal™ RE939CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: Borseal™ RE939CF is designed for: Food packaging,.. |
|||
Dart Drop, Total Energy | 30.0 J @Thickness 0.0500 mm |
22.1 ft-lb @Thickness 0.00197 in |
1100N; ISO 7765-2 |
Borealis Bormed™ RD808CF Polypropylene Random Copolymer Bormed™ RD808CF is a random copolymer. Applications: Bormed™ RD808CF is intended for packaging for medical devices, thin pouches, and packaging for pharmaceutical products. Additives: Bormed™ R.. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY CR7500 ASA High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |