Material Notes:
Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulation material for offshore deep water flow lines.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.700 g/cc
0.0253 lb/in³
ISO 1183
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.0 MPa
1600 psi
At 50 mm/min; ISO 527-2
Elongation at Break >= 50 %
>= 50 %
50 mm/min; ISO 527-3
Tensile Modulus 2.00 GPa
290 ksi
At 1 mm/min; ISO 178
Compressive Strength 17.0 MPa
2470 psi
5% Compression; ASTM D695
Thermal Properties Metric English Comments
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
ASTM C 177
Vicat Softening Point 148 °C
298 °F
A (10 N); ISO 306
Processing Properties Metric English Comments
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Melt Temperature 225 - 235 °C
437 - 455 °F
Head Temperature 220 - 230 °C
428 - 446 °F