Borealis Borcell™ HE1105 High Density Polyethylene Compound for Gas Injection of Cellular Coaxial Cables

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Borealis
Trade Name Borcell™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borcell™ HE1105 High Density Polyethylene Compound for Gas Injection of Cellular Coaxial Cables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borcell HE1105 is a high-density polyethylene (HDPE) compound formulated with specific viscosity and melt strength characteristics. Borcell HE1105 is intended for the insulations of coaxial cables using gas foaming processes and is suitable for constructions exceeding 10-mm diameter over the dielectric.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
ASTM D792
Oxidative Induction Time (OIT) 30 min
30 min
At 200°C; ASTM D3895
Melt Index of Compound 3.3 g/10 min
3.3 g/10 min
ASTM D1238/E
Electrical Properties Metric English Comments
Dielectric Constant 2.05

@Frequency 1.80e+10 Hz
2.05

@Frequency 1.80e+10 Hz
Borealis Test
2.24

@Frequency 3.00e+9 Hz
2.24

@Frequency 3.00e+9 Hz
Borealis Test
2.25

@Frequency 1e+9 Hz
2.25

@Frequency 1e+9 Hz
Borealis Test
2.33

@Frequency 1e+6 Hz
2.33

@Frequency 1e+6 Hz
Borealis Test
Dielectric Loss Index 0.000013
0.000013
At 3 GHz; Borealis Test
0.000014
0.000014
At 1 GHz; Borealis Test
0.000016
0.000016
At 18 GHz; Borealis Test
0.000080
0.000080
At 1 MHz; Borealis Test