Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 3.3 g/10 min | 3.3 g/10 min | ASTM D1238/E |
Borealis Borcell™ HE1105 High Density Polyethylene Compound for Gas Injection of Cellular Coaxial Cables Borcell HE1105 is a high-density polyethylene (HDPE) compound formulated with specific viscosity and melt strength characteristics. Borcell HE1105 is intended for the insulations of coaxial cables .. |
|||
Melt Index of Compound | 3.3 - 4.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 - 4.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group OREVAC® 9309 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |