Bayshore Vinyl Compounds BVC 4200-90 Vinyl Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Bayshore Vinyl Compounds
Trade Name BVC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bayshore Vinyl Compounds BVC 4200-90 Vinyl Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Bayshore Vinyl Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 93

@Time 10.0 sec
87 - 93

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 18.6 MPa
2700 psi
ASTM D638
Elongation at Break 290 %
290 %
ASTM D638
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D638