Mechanical Properties Metric English Comments
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-550D Solid Polyurethane Elastomer
TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
Lubrizol Estane® ALR E60D Thermoplastic Polyurethane
Type: Estane® ALR E60D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection..
100% Modulus 0.0152 GPa
2.20 ksi
Colorite Polymers Self Frosting™ 9011SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D638
Colorite Polymers 9000 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0152 GPa
2.20 ksi
Colorite Polymers 9011 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
100% Modulus 0.0152 GPa
2.20 ksi
Colorite Polymers 9012 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D638
Colorite Polymers 9033 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D638
Colorite Polymers 9034 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D638
Colorite Polymers 9226 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D-638
Axiall 35551 Wire & Cable Flexible PVC
TW, THW insulation compound suitable for 105°C AWM applications. Oil II rated and VW-1. CSA approved for TR64, TR32, TEW, and AW.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D-638
Axiall 8950 Moldings & Extrusions Flexible PVC
General purpose semi-rigid extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer
EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D638
Bayshore Vinyl Compounds BVC 4200-90 Vinyl Compound
Information Provided by Bayshore Vinyl Compounds Inc.
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D-638
Axiall 19890 Wire & Cable Flexible PVC
Highly recommended for 105°C, 15 mil wall insulations and jackets where good gasoline and oil resistance is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea
ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D-638
Axiall 22912 Coax & Telecom Flexible PVC
Non-lead stabilized, 75C rated jacket compound suitable for CM, CL2 constructions over HDPE primaries. Also suitable for riser applications over FR PVC primaries.Information provided by Georgia Gul..
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D-638
Axiall 8911 Moldings & Extrusions Flexible PVC
General purpose extrusion and molding compound. UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.