Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2180 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180 is a 80 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2180 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2180G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180G is a 80 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2180G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible G92D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV 3432 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This product has received full compliance certification for USP Biological Reactivity Tests under USP Plastic Class VI.NOTE: All ingredients used in the formulation of this compound are listed in th.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3432 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3856 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
Ineos R01A-00 Polypropylene Random Copolymer Random copolymer R01A-00 is an antistatic polypropylene produced by a unique catalyst technology. It is designed for blow molding and extrusion applications and exhibits good stiffness and improved .. |
|||
Tensile Strength at Break | 18.6 - 20.7 MPa | 2700 - 3000 psi | |
ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive , high toughness.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
Ineos R05C-00 Polypropylene Random Copolymer Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and imp.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 3710-85NT1 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Medical/Healthcare Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 4107 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 77-W280B-9 Polyvinyl Chloride, Flexible Notes: 60°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D412 |
Teknor Apex MF 165 NT Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 716 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Features: High Heat Resistance Uses: Wire and Cable Applications; Flexible Cord Insulation; Wire JacketingForms: Pellets Wire Types: SPT-1; SPT-2; SPT-3 Ag.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex Synres® SR 4336 Polypropylene Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection .. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D412 |
Teknor Apex Telcar® TL-101 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D3759 |
3M 5700 Safety Stripe Tape 3M™ Safety Stripe Tapes are durable vinyl tapes used to identify and mark traffic areas and physical hazards.Information provided by 3M |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D3759 |
3M 5702 Safety Stripe Tape 3M™ Safety Stripe Tapes are durable vinyl tapes used to identify and mark traffic areas and physical hazards.Information provided by 3M |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R350AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |