SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grades in various applicationsGood insulation valuesOutstanding bonding properties within max. service temperature rangeWater-retentive properties for quick and easy laying of dry bricks/blocks/slabs.Combined air and heat-setting.Information provided by Skamol.
Physical Properties Metric English Comments
Bulk Density 1.30 g/cc
0.0469 lb/in³
As Supplied
1.60 g/cc
0.0579 lb/in³
Dried at 110°C (230°F)
Loss On Ignition 4.10 %

@Temperature 1025 °C
4.10 %

@Temperature 1877 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1150 °C
2100 °F
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
CaO 0.40 %
0.40 %
Fe2O3 1.2 %
1.2 %
K2O 1.6 %
1.6 %
MgO 0.90 %
0.90 %
Na2O 3.6 %
3.6 %
SiO2 46 %
46 %
TiO2 1.5 %
1.5 %
Processing Properties Metric English Comments
Moisture Content 2.0 %
2.0 %
as supplied
Descriptive Properties Value Comments
Binder Silicate
Mixing Water Usage 6.8 liters to 25 kg
Package Weight 25 kg
Unit weight, all included. Plastic sack with dry mix.
Pyrometric Cone Equivalent 1585°C
ASTM C24-89, ORTON cones
Recommended Joint Thickness 3.0-5.0 mm
Setting Mechanism air and heat-setting
Type dry mix
Usage 110 kg
Quantity to set 1m<sup>3</sup> (35.31 ft<sup>3</sup>) of Bricks
5.33 kg
Quantity to fix 1m<sup>2</sup> (11 ft<sup>2</sup>) of Slabs