Polymer Property : Flexural Yield Strength = 73.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 73.1 MPa
10600 psi
ASTM D790
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Yield Strength 73.1 MPa
10600 psi
ASTM D790
PTS Trilac® ABS-HS6500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Yield Strength 73.1 MPa
10600 psi
ASTM D790
Bayshore Vinyl Compounds BRC R409002 Molding Compound
BRC 409002 is a medium impact high flow injection molding compound designed for ease of process along with excellent weathering characteristics.Information Provided by Bayshore Vinyl Compounds Inc.