Thermal Properties Metric English Comments
Heat Distortion Temperature 65.0 - 76.0 °C
149 - 169 °F
Average value: 73.5 °C Grade Count:24
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Heat Distortion Temperature >= 65.0 °C
>= 149 °F
ASTM D 648
Karina E 854-35/9-A-ERYB Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature 65.0 °C
149 °F
ASTM D648
Bayshore Vinyl Compounds BRC R409002 Molding Compound
BRC 409002 is a medium impact high flow injection molding compound designed for ease of process along with excellent weathering characteristics.Information Provided by Bayshore Vinyl Compounds Inc.