BASF Pluracol® 593 Specialty Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 593 Specialty Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 593 polyol is a 3650 molecular weight polyol containing a high proportion of ethylene oxide in the polyol chain. Pluracol 593 can be used in the formulation for hydrophillic flexible slabstock foams. Pluracol 593 is incompatible with other slab polyols and will separate from other polyols unless continuously agitated.Information provided by BASF
Physical Properties Metric English Comments
Density 1.07 g/cc

@Temperature 65.6 °C
0.0387 lb/in³

@Temperature 150 °F
1.08 g/cc

@Temperature 43.3 °C
0.0390 lb/in³

@Temperature 110 °F
1.09 g/cc

@Temperature 25.0 °C
0.0394 lb/in³

@Temperature 77.0 °F
Viscosity 183 cP

@Temperature 65.6 °C
183 cP

@Temperature 150 °F
400 cP

@Temperature 43.4 °C
400 cP

@Temperature 110 °F
1340 cP

@Temperature 25.0 °C
1340 cP

@Temperature 77.0 °F
Molecular Weight 3650 g/mol
3650 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Water White Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 44.0 - 47 mg KOH/g
STI 3007/3162
Unsaturation <0.09 meq/g
STI 3056