Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.08 - 1.11 g/cc @Temperature 20.0 °C |
0.0390 - 0.0401 lb/in³ @Temperature 68.0 °F |
A Grade, 2nd Quality |
Kazanorgsintez Purified Polyglycol Production Method: A Grade - Glycol solution in water with mass fraction greater than 75% B Grade - Glycol solution in water with mass fraction greater than 45% Application: A Grade - Intended for .. |
|||
Density | 1.08 g/cc @Temperature 100 °C |
0.0390 lb/in³ @Temperature 212 °F |
|
Solvay Chemicals Epichlorohydrin Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli.. |
|||
Density | 1.08 g/cc @Temperature 22.0 °C |
0.0390 lb/in³ @Temperature 71.6 °F |
EN542 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |
|||
Density | 1.08 g/cc @Temperature 43.3 °C |
0.0390 lb/in³ @Temperature 110 °F |
|
BASF Pluracol® 593 Specialty Polyol Description: Pluracol® 593 polyol is a 3650 molecular weight polyol containing a high proportion of ethylene oxide in the polyol chain. Pluracol 593 can be used in the formulation for hydrophillic .. |
|||
Density | 1.08 g/cc @Temperature 25.0 °C |
0.0390 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 922 Rigid Polyol Description: Pluracol® 922 polyol is an aromatic initiator-based polyol for rigid foams developed for use in spray formulations, or in polyol blends that can utilize its inherent fast reactivity. P.. |
|||
Density | 1.08 g/cc @Temperature 40.0 °C |
0.0390 lb/in³ @Temperature 104 °F |
|
BASF Pluracol® SG-370 Rigid Polyol Description: Pluracol® SG-370 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-370 contains no nitrogen. The high sucrose content without nitrogen, when combined with suitabl.. |
|||
Density | 1.08 g/cc @Temperature 25.0 °C |
0.0390 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® SG-360 Rigid Polyol Description: Pluracol® SG-360 polyol is a clear, light colored, low viscosity, sucrose/glycerine polyol. Pluracol SG-360 contains no nitrogen. The medium functionality polyol, when combined with su.. |