Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.07 g/cc @Temperature 65.6 °C |
0.0387 lb/in³ @Temperature 150 °F |
|
BASF Pluracol® 593 Specialty Polyol Description: Pluracol® 593 polyol is a 3650 molecular weight polyol containing a high proportion of ethylene oxide in the polyol chain. Pluracol 593 can be used in the formulation for hydrophillic .. |
|||
Density | 1.07 g/cc @Temperature 40.0 °C |
0.0387 lb/in³ @Temperature 104 °F |
|
BASF Pluracol® 922 Rigid Polyol Description: Pluracol® 922 polyol is an aromatic initiator-based polyol for rigid foams developed for use in spray formulations, or in polyol blends that can utilize its inherent fast reactivity. P.. |
|||
Density | 1.07 g/cc @Temperature 60.0 °C |
0.0387 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® SG-370 Rigid Polyol Description: Pluracol® SG-370 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-370 contains no nitrogen. The high sucrose content without nitrogen, when combined with suitabl.. |