Polymer Property : Viscosity = 2950 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2950 cP

@Temperature 25.0 °C
2950 cP

@Temperature 77.0 °F
BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol
Description: Pluracol® 4850 polyol is a primary hydroxyl-terminated graft polyether triol containing approximately 32% solids of copolymerized styrene and acrylonitrile, utilizing a LVI inhibitor p..