Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.04 g/cc @Temperature 40.0 °C |
0.0376 lb/in³ @Temperature 104 °F |
Concentration 0.10 kg HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |
|||
Density | 1.04 g/cc @Temperature 25.0 °C |
0.0376 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 1365 Graft Slabstock Foam Polyol Description: Pluracol® 1365 polyol is a graft polyether polyol containing copolymerized styrene and acrylonitrile. This low functionality polyol is designed to produce flexible slabstock foams with.. |
|||
Density | 1.04 g/cc @Temperature 30.0 °C |
0.0376 lb/in³ @Temperature 86.0 °F |
|
BASF Pluracol® 1365 Graft Slabstock Foam Polyol Description: Pluracol® 1365 polyol is a graft polyether polyol containing copolymerized styrene and acrylonitrile. This low functionality polyol is designed to produce flexible slabstock foams with.. |
|||
Density | 1.04 g/cc @Temperature 25.0 °C |
0.0376 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 4800 HR Foam Polyol Description: Pluracol® 4800 polyol is a primary OH tipped copolymer polyol containing approximately 45% copolymerized styrene-acrylonitrile suitable for molded foam applications. Pluracol polyol 48.. |
|||
Density | 1.04 g/cc @Temperature 40.0 °C |
0.0376 lb/in³ @Temperature 104 °F |
|
BASF Pluracol® 4800 HR Foam Polyol Description: Pluracol® 4800 polyol is a primary OH tipped copolymer polyol containing approximately 45% copolymerized styrene-acrylonitrile suitable for molded foam applications. Pluracol polyol 48.. |
|||
Density | 1.04 g/cc @Temperature 25.0 °C |
0.0376 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol Description: Pluracol® 4850 polyol is a primary hydroxyl-terminated graft polyether triol containing approximately 32% solids of copolymerized styrene and acrylonitrile, utilizing a LVI inhibitor p.. |
|||
Density | 1.04 g/cc @Temperature 40.0 °C |
0.0376 lb/in³ @Temperature 104 °F |
|
BASF Pluracol® 736 Rigid Polyol Description: Pluracol® 736 polyol is an aromatic initiator-based polyol which can be used in a variety of rigid foam formulations. This polyol can be reacted with crude MDI, crude TDI or TDI quasip.. |
|||
Density | 1.04 g/cc @Temperature 37.8 °C |
0.0376 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® GP 430R Specialty Polyol Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure.. |
|||
Density | 1.04 g/cc @Temperature 40.0 °C |
0.0376 lb/in³ @Temperature 104 °F |
|
BASF Pluracol® 5250 Graft Slabstock Foam Polyol Description: Pluracol® 5250 polyol is a graft polyether triol containing copolymerized styrene and acrylonitrile. This secondary hydroxyl-terminated polyol contains approximately 50% solids. It is .. |
|||
Density | 1.04 g/cc @Temperature 25.0 °C |
0.0376 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® GP 730 Specialty Polyol Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure.. |